Title: Examination of water phase transitions in Loblolly pine and cell wall components by differential scanning calorimetry

Source: Thermochimica Acta, 533 (2012) 39-45. 10.1016/j.tca.2012.01.015

Author(s)Zelinka, Samuel L.; Lambrecht, Michael J.; Glass, Samuel V.; Wiedenhoeft, Alex C.; Yelle, Daniel J.

Publication Year: 2012  View PDF » Mail this web page's link »

Publication Series: Journal Articles
Associated Research Project(s):   FPL-4707-3A  FPL-4714-1A  FPL-4723-1

Abstract: This paper examines phase transformations of water in wood and isolated wood cell wall components using differential scanning calorimetry with the purpose of better understanding "Type II water" or "freezable bound water" that has been reported for cellulose and other hydrophilic polymers. Solid loblolly pine (Pinus taeda) milled pine, and holocellulose, cellulose, and lignin isolated from the same parent board were tested. For each sample preparation, the freezing and melting of water was examined at 10?20 different moisture contents. Only one freezing peak was observed for most sample preparations; in these cases, the phase transformation corresponded to the "Type I" or "free water" peak. The freezing and melting temperatures of this Type I peak depended on moisture content, and appreciable undercooling (?30 °C from bulk water) was observed at the lowest moisture contents. The isolated ball-milled cellulose exhibited a Type II peak, yet the Wiley-milled cellulose, from which the ball-milled cellulose was made, did not exhibit a Type II peak. When present, the Type II peak is consistent with the homogeneous nucleation temperature of bulk water. The results suggest that the detection of Type II or freezable bound water in wood may depend more on sample preparation than the chemical nature of the cell wall component in question; a point not discussed by previous researchers describing Type II water in hydrophilic polymers.

Keywords: Differential scanning calorimetry (DSC); Wood; Cellulose; Wood?water relations; Thermodynamics; Sorption

Publication Review Process: Formally Refereed

File size: 568 kb(s)

Date posted: 04/19/2012

This publication is also viewable on Treesearch:  view
RITS Product ID: 41912
Current FPL Scientists associated with this publication (listed alphabetically)
Glass, Samuel V.
Research Physical Scientist
Wiedenhoeft, Alex C.
Research Botanist
Yelle, Daniel
Research Forest Products Technologist
Zelinka, Samuel L.
Materials Research Engineer
  

Additional items that might interest you


2011 Research Highlights from FPL....view



2010 Research Highlights from FPL....view



Termite Eradication: A search for the Holy Grail.... view



Moisture Management in Residential Construction Series videos...view


Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »