Title: An experimental study on swelling of cellulose nano-fiber films in epoxy resins and water

Source: SAMPE 2011 [electronic resource] : May 23-26, 2011, Long Beach, CA. [Covina, CA] : Society for the Advancement of Material and Process Engineering, c2011: 9 p.

Author(s)Masoodi, R.; Javadi, A.; Pillai, K.M.; Sabo, Ronald

Publication Year: 2011  View PDF » Mail this web page's link »

Publication Series: Conference Proceedings
Associated Research Project(s):   FPL-4706-1A

Abstract: The current breed of natural-fiber based polymer composites, because of their biobased and possibly biodegradable nature, offer an alternative as a `green? material available for automotive and other engineering applications. However such composites suffer from the drawback of low strength and fatigue properties compared to the carbon- or glass-fiber based polymer composites. Cellulose nanofibers (CNFs) are a new type of nanofibers made purely from cellulose molecules and have very high mechanical properties compared to other natural fibers, even approaching that of inorganic reinforcing fibers. However, there remain several hurdles in the use of CNF films for the production of polymer composites through the liquid composite molding technologies. One such problem is the swelling of these films during the manufacturing of such composites. In this study, we have microscopically studied the swelling of CNF films when they come in contact with three different liquids: water, epoxy, and bio-based epoxy. It was observed that the swelling rate was very high in the beginning but decreased subsequently. The swelling process was seen to be complete within two minutes for all the three liquids. The highest and lowest swelling of CNF films were observed for water and bioepoxy, respectively.

Keywords: Nanofibers, cellulose, nanotechnology, cellulose fibers, composite materials, nanocomposites, mechanical properties, adsorption, nanostructured materials, moisture, thin films, fatigue, epoxy resins, nanocellulose, cellulose nanofibers, biocomposites, swelling, polymers, polymerization, strength

Publication Review Process: Non-Refereed (Other)

File size: 488 kb(s)

Date posted: 09/27/2011

This publication is also viewable on Treesearch:  view
RITS Product ID: 40103
Current FPL Scientist associated with this publication
Sabo, Ronald C.
Research Materials Engineer
  

Additional items that might interest you


2011 Research Highlights from FPL....view



2010 Research Highlights from FPL....view



Termite Eradication: A search for the Holy Grail.... view



Moisture Management in Residential Construction Series videos...view


Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »