Title: Heat of combustion of various southern pine materials

Author: Howard, E.T.

Date: 1973

Source: Wood Science 5(3):194-197

Description: As measured with an oxygen-bomb calorimeter, heats of combustion averaged about 8,600 Btu/ovendry lb. for stemwood, rootwood, earlywood, and latewood. In stemwood, 54 percent of the variation was related to extractive content. Values for bark were greatest in samples from the base of the tree and decreased with increasing height in tree. Values for resinous wood varied directly with extractive content. Needles and mixed bark had higher heats of combustion than stemwood. Spruce pine bark produced less heat than mixed bark from the other southern pine species. Samples from tops had lower values than other woody portions; of aU tree parts, old cones ranked lowest. Dried kraft black liquor averaged only 5,965 Btu/ovendry lb.

Keywords: 

View and Print this Publication (630 KB)

Publication Notes: 

  • We recommend that you also print this page and attach it to the printout of the article, to retain the full citation information.
  • This article was written and prepared by U.S. Government employees on official time, and is therefore in the public domain.

 [ Get Acrobat ]  Get the latest version of the Adobe Acrobat reader or Acrobat Reader for Windows with Search and Accessibility

Citation

Howard, E.T.  1973.  Heat of combustion of various southern pine materials.   Wood Science 5(3):194-197

US Forest Service - Research & Development
Last Modified:  January 16, 2009


USDA logo which links to the department's national site. Forest Service logo which links to the agency's national site.