Fiber Processing & Paper Performance
FS-FPL-4710
Wood Reduction |
- Chipper -- 4 bladeProduction
of pulping chips, 6.4-19mm
- Classification
--
- Shaker (bulk) -- Sizing of chips,etc.(used with chipper) a wide variety
of screen sizes and shapes are available
- Chip Mixer -- Twin Shell V Mixer
- Pulping --
- Digesters (batch) -- Small
scale cooks; 23L, stainless steel, 2-2.5kg ovendry; 3 stationary and one rotating
- Digesters (batch) -- Intermediate cooks: 368 and 396 L, 65kg ovendry; rotating
- Digesters (batch) -- Large cooks : 2800L, stainless steel, 225kg ovendry: stationary
- Fiber Processing
--
- Refiner (Pressurized) --
Production of TMP & CTMP, 30-cm stainless steel, 150 psig, maximum
pressure. 50L
- Refiners (Atmospheric) -- Fiberizing of chips after pulping, 20 cm.
- Refiner (Atmospheric) -- High-volume, 90 cm, double counter rotating disk.
- Refiner (Atmospheric) -- High-Volume use, 55 cm, single rotating disk.
|
Pulp Processing and Recycling |
- Pulpers --
For repulping of paper; low (3%-6%), medium (7%-12%) and high consistency
(>12%).
- Low and medium consistency 25 and 100 kg capacities.
- High consistency, 50L
and 1500 Liter capacities.
- Flatscreens
--
- High-volume large-particle separation,0.10, 0.20 and 0.30-mm slots,
1.02m by 1.83m usable area.
- Medium-sized batch operation, 0.20 and 0.275 mm slots,1.04m
by 0.58m usable area.
- Small 250 by 300 mm, 0.1-0.5 mm, slotted screens
available.
- Pressure
screens
--
- Coarse and fine, 0.3, 0.2, 0.10 and 0.15 mm; light-weight particle removal.
- Large-scale heavy-weight particle removal, low consistency (1%, continuous use, 3 baskets available (0.26 and 0.30
mm slots, 1.6 mm holes.
- Centricleaners --
75 and 150mm forward cleaners.
Flow through cleaners two types, both 75 mm.
- Flotation unit -- Large-scale
deinking, batch or continuous.
- Flotation unit (Denver cell) --
Single-batch bench-scale deinking, 90-L single cell unit with stirrer
and air injection.
- Flotation unit -- Large-scale
deinking, continuous, 6 cells in series.
- Sidehill screen --
70-mesh wire, 0.7m by 1.73m surface.
- Hydrosieve -- Horizontal
slots of 0.25, 0.75, or 1.5mm, 0.5m by 0.46m area.
- Centrifuge -- Small-scale dewatering, max output consistency of 40%.
- Bladder press (2) -- Small
scale dewatering, batch units, consistencies up 40%.
- Drum washer -- Large-scale dewatering, continuous
input, 900 mm diameter, 300 mm wide vacuum drum with shredder.
|
Paper Production |
- Paper
machine -- Lab-scale paper and fiberboard production, 450-mm wire,
300-mm web, normal width due to headbox and calendar size, minimum
speed 1 m/min, maximum speed 30m/min, hydrapulper and refiners available
for
stock preparation
- Pulp Processing
Wet Lab -- Pulpsheet preparation, small-scale beater, 2 TAPPI
PFI mills (1 equipped with variable speed drive),handsheet former,
freeness
testers, balances dryers etc.
- Clarifier --
Water clarifier for recycling operations closed loop system
- Cytec
Metering System -- Chemical metering station for clarifier
- PIRA
Sticky Disposition Analyzer -- Two stage system for separating
stickies from a slurry and then measuring quantity by image
analysis.
|