Publication Information
Title: Continuous tunnel kiln direct-fired with bark to dry 1.75-inch southern pine in 12 hours.
Author: Koch, P.; Wellford, W.L.
Date: 1977
Source: Forest Products Journal 27(5):39-47
Description: Length-sorted lumber is surfaced on one side to 1.75-inch thickness, mechanically stacked 5 feet wide and 10 feet high on 1-1/4-inch-thick sticks, and continuously transported through a zone-controlled tunnel kiln at 8 ft./hr. to yield 500,000 fbm of lumber dried to 9 percent average MC per 168-hour week. In the tunnel, the lumber is dried for 8 (possibly 10) hours at 270°F, conditioned for 3 hours at 195°F, and cooled for 1 hour before discharge to cooling sheds and subsequent unstacking. During drying and conditioning, wetbulb temperature is held constant at 185°F. Air velocities
vary by zone; i.e., 1,600 fpm at inlet, 300 fpm while conditioning, and 1,000 fpm while cooling. To control warp, a top load (12 in. of concrete) is automatically placed on the moving lumber stacks as they enter the tunnel kiln and removed as they exit.
Keywords:
View and Print this Publication (2.1 MB)
Publication Notes:
- We recommend that you also print this page and attach it to the printout of the article, to retain the full citation information.
- This article was written and prepared by U.S. Government employees on official time, and is therefore in the public domain.
Get the latest version of the Adobe Acrobat reader or Acrobat Reader for Windows with Search and Accessibility
Citation
Koch, P.; Wellford, W.L. 1977. Continuous tunnel kiln direct-fired with bark to dry 1.75-inch southern pine in 12 hours.. Forest Products Journal 27(5):39-47
|