This publication is in Portable Document Format (PDF--Adobe Acrobat). These files may be downloaded (for viewing or printing) by clicking on the linked titles. The Adobe Acrobat Reader (version 4.0 or later) must be installed on your system to view or print a PDF document. The Acrobat Reader may be part of your Web browser, or you may download it free.
 

Wood Handbook
Wood as an engineering material. General Technical Report 113.
Madison, WI: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 463 p.


Front matter (PDF 292 KB)

  • Preface
  • Acknowledgments
  • Contributors

Chapter 1 -- Characteristics and Availability of Commercially Important Wood (PDF 916 KB)

  • Timber Resources and Uses
  • Species Descriptions
  • U.S. Wood Species
  • Imported Woods

Chapter 2 -- Structure of Wood (PDF 434 KB)

  • Bark, Wood, Branches, and Cambium
  • Sapwood and Heartwood
  • Growth Rings
  • Wood Cells
  • Chemical Composition
  • Species Identification

Chapter 3 -- Physical Properties and Moisture Relations of Wood (PDF 495 KB)

  • Appearance
  • Moisture Content
  • Shrinkage
  • Weight, Density, and Specific Gravity
  • Working Qualities
  • Decay Resistance
  • Thermal Properties
  • Electrical Properties
  • Coefficient of Friction
  • Nuclear Radiation

Chapter 4 -- Mechanical Properties of Wood (PDF 1.2 MB)

  • Orthotropic Nature of Wood
  • Elastic Properties
  • Strength Properties
  • Vibration Properties
  • Mechanical Properties of Clear Straight-Grained Wood
  • Natural Characteristics Affecting Mechanical Properties
  • Effects of Manufacturing and Service Environments

Chapter 5 Commercial Lumber (PDF 551 KB)

  • Hardwood Lumber
  • Softwood Lumber
  • Purchase of Lumber
  • Commonly Used Lumber Abbreviations

Chapter 6 -- Lumber Stress Grades and Design Properties (PDF 329 KB)

  • Responsibilities and Standards for Stress Grading
  • Visually Graded Structural Lumber
  • Machine-Graded Structural Lumber
  • Adjustment of Properties for Design Use

Chapter 7 -- Fastenings (PDF 1.1 MB)

  • Nails
  • Spikes
  • Staples
  • Drift Bolts
  • Wood Screws
  • Lag Screws
  • Bolts
  • Connector Joints
  • Multiple-Fastener Joints
  • Metal Plate Connectors
  • Fastener Head Embedment

Chapter 8 -- Structural Analysis Equations (PDF 320 KB)

  • Deformation Equations
  • Stress Equations
  • Stability Equations

Chapter 9 -- Adhesive Bonding of Wood Materials (PDF 433 KB)

  • Adhesion to Wood
  • Surface Properties of Wood Adherends
  • Physical Properties of Wood Adherends
  • Adhesives
  • Bonding Process
  • Bonded Joints
  • Testing and Performance

Chapter 10 -- Wood-Based Composites and Panel Products (PDF 904 KB)

  • Scope
  • Types of Conventional Composite Materials
  • Adhesive Considerations
  • Additives
  • General Manufacturing Issues
  • Standards for Wood-Based Panels
  • Plywood
  • Particle and Fiber Composites
  • Wood-Nonwood Composites

Chapter 11 -- Glued Structural Members (PDF 975 KB)

  • Structural Composite Lumber
  • Glulam
  • Glued Members With Lumber and Panels
  • Structural Sandwich Construction

Chapter 12 -- Drying and Control of Moisture Content and Dimensional Changes (PDF 1.3 MB)

  • Determination of Moisture Content
  • Recommended Moisture Content
  • Drying of Wood
  • Moisture Control During Transit and Storage
  • Dimensional Changes in Wood
  • Design Factors Affecting Dimensional Change
  • Wood Care and Installation During Construction

Chapter 13 -- Biodeterioration of Wood (PDF 599 KB)

  • Fungus Damage and Control
  • Bacteria
  • Insect Damage and Control
  • Marine Borer Damage and Control

Chapter 14 -- Wood Preservation (PDF 1.2 MB)

  • Wood Preservatives
  • Preservative Effectiveness
  • Effect of Species on Penetration
  • Preparation of Timber for Treatment
  • Application of Preservatives
  • Handling and Seasoning of Timber After Treatment
  • Quality Assurance for Treated Wood

Chapter 15 -- Finishing of Wood (PDF 2.2 MB)

  • Factors Affecting Finish Performance
  • Control of Water or Moisture in Wood
  • Types of Exterior Wood Finishes
  • Application of Wood Finishes
  • Finish Failure or Discoloration
  • Finishing of Interior Wood
  • Finishes for Items Used for Food
  • Wood Cleaners and Brighteners
  • Paint Strippers
  • Lead-Based Paint 15-35

Chapter 16 -- Use of Wood In Building and Bridges (PDF 779 KB)

  • Light-Frame Buildings
  • Post-Frame and Pole Buildings
  • Log Buildings
  • Heavy Timber Buildings
  • Timber Bridges
  • Considerations for Wood Buildings

Chapter 17 -- Fire Safety (PDF 318 KB)

  • Fire Safety Design and Evaluation
  • Fire Performance Characteristics of Wood
  • Flame-Retardant Treatments

Chapter 18 -- Round Timbers and Ties (PDF 396 KB)

  • Standards and Specifications
  • Material Requirements
  • Availability
  • Form
  • Weight and Volume
  • Durability
  • Strength Properties

Chapter 19 -- Specialty Treatments (PDF 298 KB)

  • Plasticizing Wood
  • Modified Woods
  • Paper-Based Plastic Laminates

Glossary (PDF 178 KB)

Index (PDF 154 KB)

| Important Notices | FOIA | Privacy Notice | Quality of Information | Site Map | Site Help |